Tiling mortars

Masonry Mortar High Performance
Use

For jointing AAC (Autoclaved Aerated Concrete) and lightweight blocks.

Compressive Strength

>10 N/sq.mm.

Consumption

1.7-2.1 kg/sq.m/mm.

Bag Size

25 kg and 40 kg.

Micro Mortar
Use

For restrengthening superstructures of variable strength during repairs and rehabilitation work.

Compressive Strength

7 Days: 25 MPa, 28 Days: 35 MPa

Consumption

2.2-2.4 kg/sq.m/mm.

Bag Size

25 kg.

Renovation Mortar
Use

For restrengthening superstructures of variable strength during repairs and rehabilitation work.

Compressive Strength

3 Days: 30 MPa, 7 Days: 45 MPa, 28 Days: 60 MPa

Consumption

2.2-2.4 kg/sq.m/mm.

Bag Size

25 kg.

Super Tile Mortar
Use

For durable tile work of large vitrified tiles, marbles, decorative stones, and tile-on-tile work.

Compressive Strength

>10 N/sq. mm.

Consumption

1.15 Kg/sq. m/mm.

Bag Size

20 & 25 Kg.